川西某锂多金属矿选矿试验研究

谭 华1 费光春2 蔡云华1 谭 心2 杨贵兵1 朱汇派1 李 剑1   

  1. 1. 四川省综合地质调查研究所,四川 成都 618000;2. 成都理工大学地球与行星科学学院,四川 成都 610059
  • 出版日期:2026-03-15 发布日期:2026-03-31
  • 通讯作者: 费光春(1982—),男,教授,博士,硕士研究生导师。
  • 作者简介:谭 华(1975—),男,高级工程师。
  • 基金资助:
    四川省政府性投资地质勘查项目(编号:DZ202414);四川省地质调查研究院科研项目(编号:SCLGS-CZDXM-2024001)。

Experimental Study on Mineral Dressing of a Lithium Polymetallic Ore in Western Sichuan

TAN Hua1 FEI Guangchun2 CAI Yunhua1 TAN Xin2 YANG Guibing1 ZHU Huipai1 LI Jian1   

  1. 1. Sichuan Institute of Comprehensive Geological Survey,Chengdu 618000,China;
    2. College of Earth and Planetary Science,Chengdu University of Technology,Chengdu 610059,China
  • Online:2026-03-15 Published:2026-03-31

摘要: 四川西部某伟晶岩型低品位锂多金属矿主要可回收利用矿物为锂辉石,同时伴生少量铌钽矿物,其
Li2O、Nb2O5 和Ta2O5 品位分别为1. 25%、0. 009%、0. 003%。为高效综合利用该矿石资源,在磨矿细度为-0. 074 mm
占74. 3%的条件下,采用锂辉石捕收剂EM-PN30,在1 粗2 扫3 精浮选闭路流程情况下进行试验。最终获得了含铌钽
锂精矿,Li2O、Nb2O5 和Ta2O5 品位分别为5. 60%、0. 035%、0. 015%,回收率分别为86. 31%、75. 52%、72. 82%。再经强
磁—重选试验,分离出Li2O 品位为5. 65%的锂精矿和(Nb2O5 +Ta2O5 )品位为30. 23%的铌钽精矿。采用“锂铌钽混
浮—混浮精矿弱磁除铁—强磁选—重选分离”的工艺流程不仅能够充分回收矿石中的锂,获得指标较为理想的锂精
矿,还能分离回收得到铌钽精矿,实现了矿石中锂、铌、钽元素的高效综合利用。

Abstract: This study focuses on the efficient recovery and utilization of a pegmatite-type low-grade lithium polymetallic
ore from western Sichuan,primarily through the extraction of spodumene,with minor amounts of niobium-tantalum minerals. The
ore grades of Li2O,Nb2O5,and Ta2O5 are 1. 25%,0. 009%,and 0. 003%,respectively. To optimize the extraction process,the
spodumene collector EM-PN30 was used,and flotation tests were conducted under the conditions of a grinding fineness of
0. 074 mm at 74. 3% passing. The flotation process,comprising one roughing,two scavenging,and three cleaning stages,successfully
produced a lithium-niobium-tantalum concentrate with grades of 5. 60% Li2O,0. 035% Nb2O5,and 0. 015% Ta2O5,
achieving recoveries of 86. 31%,75. 52%,and 72. 82%,respectively. Further separation of the lithium concentrate and niobium-
tantalum concentrate was achieved through high-intensity magnetic and gravity separation,resulting in a lithium concentrate
with a Li2O grade of 5. 65% and a niobium-tantalum concentrate containing (Nb2O5 +Ta2O5) at 30. 23%. The results indicate
that the combined process of "lithium-niobium-tantalum mixed flotation,mixed flotation concentrate low-intensity magnetic iron
removal,high-intensity magnetic separation,and gravity separation" not only ensures the efficient recovery of lithium,but also
facilitates the separation and recovery of niobium-tantalum,thus enabling the comprehensive utilization of lithium,niobium,and
tantalum from the ore.