欢迎访问《金属矿山》杂志官方网站,今天是 分享到:
×

扫码分享

金属矿山 ›› 2026, Vol. 55 ›› Issue (4): 134-139.

• 矿物工程 • 上一篇    下一篇

印度某赤铁矿石高压辊磨工艺应用研究

李 烨1 邓 洁1 孙业长2   

  1. 1. 中钢设备有限公司矿业工程部,北京 100080;2. 成都利君实业股份有限公司,四川 成都 610000
  • 出版日期:2026-04-15 发布日期:2026-05-08
  • 通讯作者: 孙业长(1964—),男,教授级高级工程师,硕士。
  • 作者简介:李 烨(1980—),男,总经理,高级经济师,硕士。

Application Research of High-Pressure Grinding Rolls Technology on a Hematite Ore in India

LI Ye1 DENG Jie1 SUN Yechang2   

  1. 1. Mining Engineering Department,Sinosteel Equipment & Engineering Co. ,Ltd. ,Beijing 100080,China;
    2. Chengdu Lijun Industrial Co. ,Ltd. ,Chengdu 610000,China
  • Online:2026-04-15 Published:2026-05-08

摘要: 为探究高压辊磨工艺在国外低品位赤铁矿中的应用效果,本文以矿山代表性赤铁矿为研究对象,系统
考察了辊面压力、矿样含水量对高压辊磨产品粒度分布、单位能耗及可磨度的影响,并结合湿式预选工艺验证了辊磨
产品的分选效果。试验结果表明,在辊面压力5. 54 N/ mm2、矿样含水量3%、筛分粒度3 mm 的条件下,闭路稳定后最
终排料-3 mm 粒级含量由9. 10%提升至49. 46%,增加40. 36 个百分点,F50 / P50 = 6. 21,辊压效果良好;闭路循环负荷
为115. 95%,单位能耗为1. 75 kWh/ t,单位处理量为280. 16 t·s/ (h·m3)。相对可磨度试验表明,高压辊磨闭路产品较
粗碎原矿更易磨,达到相同磨矿细度所需时间更短。对高压辊磨-3 mm 产品进行2 次强磁粗选,在背景磁感应强度
均为1. 4 T 条件下,可获得铁品位42. 20%、铁回收率96. 32%的综合精矿,尾矿铁品位7. 60%、尾矿产率17. 54%。研
究成果为国外低品位赤铁矿的高压辊磨工艺参数优化与磨前预选应用提供了技术依据。

关键词: 高压辊磨机 , 赤铁矿 , 粒度分布 , 湿式预选 , 可磨度

Abstract: To investigate the application performance of high-pressure grinding rolls (HPGR) technology in a low-grade
hematite ore from abroad,this study takes a representative hematite sample from the mine as the research object. The effects of
roll surface pressure and feed moisture content on the particle size distribution,specific energy consumption,and grindability of
HPGR products were systematically investigated,and the separation efficiency of the crushed products was verified through wet
pre-concentration tests. The results of closed-circuit tests with 3 mm screening show that under the conditions of roll surface
pressure of 5. 54 N/ mm2,feed moisture content of 3%,and stable operation,the -3 mm fraction in the final discharge increased
from 9. 10% to 49. 46%,an increase of 40. 36 percentage points,with an F50 / P50 ratio of 6. 21,indicating satisfactory
crushing performance. The circulating load was 115. 95%,specific energy consumption was 1. 75 kWh/ t,and specific throughput
was 280. 16 t·s/ (h·m3). Relative grindability tests indicate that the HPGR closed-circuit product (-3 mm) is more readily
grindable than the coarsely crushed ore,requiring less grinding time to achieve the same fineness. Wet pre-concentration
tests using two stages of high-intensity magnetic roughing separation at a background magnetic induction intensity of 1. 4 T yielded
a combined concentrate with an iron grade of 42. 20% and iron recovery of 96. 32%,while the tailings had an iron grade of
7. 60% with a yield of 17. 54%. The research findings provide technical support for optimizing HPGR process parameters and
implementing pre-concentration strategies for this low-grade hematite ore in abroad.

Key words: high-pressure grinding rolls (HPGR),hematite,particle size distribution,wet pre-concentration,grindability