欢迎访问《金属矿山》杂志官方网站,今天是 分享到:
×

扫码分享

金属矿山 ›› 2026, Vol. 55 ›› Issue (9): 174-181.

• 矿物工程 • 上一篇    下一篇

某含钛铁精矿工艺矿物学及提质试验研究

米宏成1 ,李丽匣1 ,胡厚勤2 ,张 春2 ,褚 洋1 ,陈家宽1 ,杨淑贤1 ,李思佑1 ,王嘉琦1   

  1. 1.东北大学资源与土木工程学院,辽宁 沈阳 110819;2.攀钢集团矿业有限公司,四川 攀枝花 617000
  • 出版日期:2026-09-15 发布日期:2026-10-15
  • 通讯作者: 李丽匣(1980—),女,教授,博士,博士研究生导师。
  • 作者简介:米宏成(1996—),男,博士研究生。
  • 基金资助:
    国家自然科学基金项目(编号:52174243);辽宁省重点研发计划项目(编号:2024 JH2/102400026)。

Study on the Process Mineralogy and Quality Improvement Test of a Titanium-Bearing Iron Concentrate

MI Hongcheng1 ,LI Lixia1 ,HU Houqin2 ,ZHANG Chun2 ,CHU Yang1 ,CHEN Jiakuan1 ,YANG Shuxian1 ,LI Siyou1 ,WANG Jiaqi1   

  1. 1.School of Resources and Civil Engineering,Northeastern University,Shenyang 110819,China; 2.Pangang Group Mining Company,Panzhihua 617000,China
  • Online:2026-09-15 Published:2026-10-15

摘要: 为进一步提升攀西地区某含钛铁精矿的铁品位,开展了工艺矿物学与细磨—磁选试验研究。通过矿物 嵌布特征与元素赋存状态分析,明确了影响精矿提质的矿物学因素,并评估了细磨提质的可行性。结果表明,样品 TFe品位为41.59%,TiO2 含量为10.84%;主要有用矿物为钛磁铁矿和钛铁矿,脉石以辉石、绿泥石、钛闪石、角闪石和 斜长石为主。铁主要赋存于磁性铁矿物中,分布率为90.12%;钛主要分布于钛磁铁矿和钛铁矿中,其中钛磁铁矿中 TiO2 分布率为65.59%。钛磁铁矿、钛铁矿和榍石均以细粒嵌布为主,且与脉石连生紧密,钛磁铁矿单体解离度仅为 36.12%,是限制铁精矿品位提升的主要因素。采用卧式搅拌磨将物料磨至-45 μm占比90%后,矿物解离度显著改 善;经两段磁选,最终获得产率78.06%、TFe品位50.90%、TFe回收率95.54%的磁选精矿,精矿中SiO2 、MgO、Al2 O3 和CaO等脉石组分明显降低。结果表明,细磨—多段磁选工艺可有效实现钛磁铁矿精矿的提质降杂,研究结果为攀 西地区钒钛磁铁矿精矿的深度提质提供了技术参考。

关键词: 含钛铁精矿 , 工艺矿物学 , 矿物组成 , 细磨 , 磁选提质

Abstract: To further improve the iron grade of a titanium-bearing iron concentrate in the Panxi area,a process mineralo gy and fine grinding-magnetic separation experimental study was conducted.Through analysis of mineral dissemination charac teristics and element occurrence states,the mineralogical factors affecting concentrate upgrading were clarified,and the feasibil ity of fine grinding for upgrading was evaluated.The results show that the sample has a TFe grade of 41.59% and a TiO2 con tent of 10.84%.The main valuable minerals are titanomagnetite and ilmenite,while the gangue minerals are mainly pyroxene, chlorite,kaersutite,hornblende,and plagioclase. Iron is mainly hosted in magnetic iron minerals,with a distribution rate of 90.12%;Titanium is mainly distributed in titanomagnetite and ilmenite,among which the TiO2 distribution rate in titanomagne tite is 65.59%.Titanomagnetite,ilmenite,and sphene are mainly finely disseminated and closely intergrown with gangue miner als.The liberation degree of titanomagnetite is only 36.12%,which is the main factor limiting the improvement of iron concen trate grade.After grinding the material to 90% passing 45 μm using a horizontal stirred mill,the mineral liberation was signifi cantly improved. Through two-stage magnetic separation,a magnetic concentrate with a yield of 78. 06%,TFe grade of 50.90%,and TFe recovery of 95.54% was obtained,and the contents of gangue components such as SiO2 ,MgO,Al2 O3 ,and CaO in the concentrate were significantly reduced.The results indicate that the fine grinding and multi-stage magnetic separa tion process can effectively upgrade and reduce impurities in titanomagnetite concentrate.This study provides a technical refer ence for the deep upgrading of vanadium-titanium magnetite concentrate in the Panxi area.

Key words: titanium-bearing iron concentrate,process mineralogy,mineral composition,fine grinding,magnetic separation upgrading

中图分类号: