欢迎访问《金属矿山》杂志官方网站,今天是 分享到:
×

扫码分享

金属矿山 ›› 2026, Vol. 55 ›› Issue (10): 162-168.

• • 上一篇    下一篇

某细粒嵌布磁铁矿石的选矿工艺研究

袁 壮   

  1. 长沙矿冶研究院有限责任公司,湖南 长沙 410012
  • 出版日期:2026-11-03 发布日期:2026-11-09
  • 作者简介:袁 壮(1994—),男,工程师,硕士。
  • 基金资助:
    “十四五”国家重点研发计划项目(编号:2022YFC2904402)。

Study on Beneficiation Process of a Fine-Grained Disseminated Magnetite Ore

YUAN Zhuang   

  1. Changsha Research Institute of Mining & Metallurgy Co.,Ltd.,Changsha 410012,China
  • Online:2026-11-03 Published:2026-11-09

摘要: 针对某细粒嵌布磁铁矿资源禀赋差、传统单一干法或湿法选矿工艺存在局限性等问题,基于详细的工 艺矿物学研究,提出了干式磁选+湿式磁选联合选别工艺。工艺矿物学研究表明,矿石TFe品位为29.00%,磁铁矿中 铁分布率仅为67.10%,含铁硅酸盐矿物中铁分布率高达27.76%;磁铁矿嵌布粒度较细,主要为0.02~0.20 mm,但多 沿解理发育的脉石粒间分布,有利于解离。原矿直接干式磁力预选抛尾,可抛出产率23.09%、mFe品位仅0.64%、 mFe损失率0.73%的尾矿;预选精矿经破碎后干式磁力粗选,又可抛出作业产率16.10%的粗选尾矿。对粗选精矿进 行干式制粉及干式磁选后,所得中矿经湿式再磨再选,最终全流程获得产率31.06%、TFe品位65.78%、mFe品位 63.69%、TFe回收率69.24%、mFe回收率98.07%的铁精矿,指标良好,且湿尾矿产率仅为2.78%。该联合工艺有效 解决了纯干选微细粒分选精度低、纯湿选水耗高的问题,实现了“能抛早抛”的显著减量效果,为细粒嵌布磁铁矿的高 效、节水型选矿提供了新的技术途径。

关键词: 细粒嵌布磁铁矿 , 干式磁选 , 湿式磁选 , 预选抛尾 , 联合工艺

Abstract: To address the challenges of poor resource endowment of a fine-grained disseminated magnetite ore and the limitations of conventional single dry or wet beneficiation processes,a combined "dry magnetic separation + wet magnetic sepa ration" process was proposed based on detailed process mineralogical studies.The process mineralogy results showed that the ore has a TFe grade of 29.00%,with only 67.10% of iron distributed in magnetite and up to 27.76% in iron-bearing silicate minerals.Magnetite is finely disseminated,predominantly in the size range of 0.02~0.20 mm,but is often distributed along the interstices of gangue minerals with well-developed cleavage,facilitating liberation.Direct dry magnetic separation of the raw ore for pre-concentration tailings discarding yielded tailings with a yield of 23.09%,mFe grade of only 0.64%,and mFe loss rate of 0.73%.After crushing,the pre-concentrated concentrate underwent dry magnetic separation roughing,which further discar ded roughing tailings with a yield of 16.10%.The roughing concentrate was subjected to dry grinding and dry magnetic separa tion,and the obtained middlings were processed by wet regrinding and re-concentration.The final closed-circuit process a chieved excellent indices with an iron concentrate yield of 31.06%,TFe grade of 65.78%,mFe grade of 63.69%,TFe recovery of 69.24%,and mFe recovery of 98.07%,while the wet tailings yield was only 2.78%.The combined process effectively over comes the low separation precision of pure dry separation for fine particles and the high water consumption of pure wet separa tion,achieving significant "early discard" effects and providing a new technical approach for efficient and water-saving benefi ciation of fine-grained disseminated magnetite ores.

Key words: fine-grained disseminated magnetite,dry magnetic separation,wet magnetic separation,pre-concentration tail ings discarding,combined process

中图分类号: