低浓度CO2 预碳化水泥废水:水泥基材料性能增强与碳利用新途径

张永强1 ,张 凡1 ,袁锋华1 ,张家更2 ,潘正良3   

  1. 1.江苏城乡建设职业学院土木工程学院,江苏 常州 213147;2.徐州市宏达土木工程试验室有限责任公司,江苏 徐州 221008; 3.扬州元益混凝土有限公司,江苏 扬州 225117
  • 出版日期:2026-11-03 发布日期:2026-11-10
  • 作者简介:张永强(1986—),男,讲师,硕士。
  • 基金资助:
    2022年第二批江苏省产学研合作项目(编号:BY20221402);江苏省高职院校青年教师企业实践项目(编号:2020QYSJ069);2023年江 苏省建设系统科技指导项目(编号:2023ZD044);江苏城乡建设职业学院“建筑材料与检测专创融合团队”资助项目(编号: YXZJ0000904);江苏省高职院校智能建造3D技术应用工程技术研究开发中心和江苏城乡建设职业学院智能建造科研平台资助项目 (编号:2023)。

Low Concentration CO2 Pre-Carbonation of Cement Wastewater:A New Route to Performance Enhancement and Carbon Utilization for Cement-Based Materials

ZHANG Yongqiang1 ,ZHANG Fan1 ,YUAN Fenghua1 ,ZHANG Jiageng2 ,PAN Zhengliang3   

  1. 1.School of Civil Engineering,Jiangsu Vocational College of Urban and Rural Construction,Changzhou 213147,China; 2.Xuzhou Hongda Civil Engineering Testing Laboratory Co.,Ltd.,Xuzhou 221008,China; 3.Yangzhou Yuanyi Concrete Co.,Ltd.,Yangzhou 225117,China
  • Online:2026-11-03 Published:2026-11-10

摘要: 为有效缓解水泥废水(CWw)对环境造成的负担,本研究提出采用低浓度CO2 对CWw进行预碳化处理, 以实现其作为拌合水在水泥基材料中的资源化利用。通过将高纯度CO2 与N2 混合,配制了CO2 体积分数分别为0、 20%、40%、60%和80%的碳化气体,对CWw进行预处理。结果表明:预碳化处理可显著缓解CWw引起的新拌水泥浆 体流动度下降过快及凝结时间缩短的问题,且改善效果随CO2 浓度升高而增强。与未处理CWw组相比,经40%和 60%的CO2 预碳化后,浆体的2 h流动度提升5.2%~10.7%,初凝时间恢复至对照组水平。预碳化过程中生成的 CaCO3 发挥孔隙填充与成核诱导的双重作用,促进了水化进程与微观结构致密化。其中,60%的CO2 预碳化处理使 28 d净浆的抗压强度较未处理CWw组提高3.5%,累计孔体积较对照组降低18.91%。综合力学性能、经济效益与环 境影响,40%~60%的CO2 为较佳预碳化浓度区间。该低浓度CO2 预碳化技术为CWw的资源化利用及低碳混凝土制 备提供了可行路径。

关键词: 水泥基材料 , 预碳化 , 水泥废水 , 二氧化碳 , 碳酸钙 , 抗压强度

Abstract: To effectively alleviate the environmental burden caused by cement wastewater (CWw),this study proposes a precarbonation treatment of CWw using low-concentration CO2 ,aiming to enable its reuse as mixing water in cement-based ma terials.By mixing highpurity CO2 with N2 ,carbonation gases with CO2 volume fractions of 0,20%,40%,60%,and 80% were prepared.The results show that precarbonation significantly mitigates the rapid loss of fluidity and the shortening of setting time of fresh cement paste,with the improvement effect increasing with CO2 concentration.Compared with the untreated CWw group, precarbonation with 40% and 60% CO2 increases the 2 h fluidity of the paste by 5.2% to 10.7% and restores the initial setting time to the level of the control group.The CaCO3 generated during precarbonation acts as pore filler and nucleation sites,pro moting hydration and microstructure densification.In particular,precarbonation with 60% CO2 increases the 28 d compressive strength of the paste by 3.5% compared with the untreated CWw group,and reduces the cumulative pore volume by 18.91% relative to the control group.Considering mechanical properties,economic benefits,and environmental impact,the optimal pre carbonation concentration range is 40%-60% CO2 .The proposed lowconcentration CO2 precarbonation technology provides a feasible pathway for the resource utilization of CWw and the production of lowcarbon concrete.

Key words: cement-based materials,precarbonation,cement wastewater,carbon dioxide,calcium carbonate,compressive strength

中图分类号: