欢迎访问《金属矿山》杂志官方网站,今天是 分享到:
×

扫码分享

金属矿山 ›› 2026, Vol. 55 ›› Issue (10): 312-320.

• 矿物材料 • 上一篇    

磷石膏地聚合物与轻质集料协同制备全固废路面基层材料及其耐久性

杨永恒1 ,马 佳1 ,邓宏亮2,3 ,纪小平2 ,董立源2 ,李勇涛1   

  1. 1.陕西交控建投经营管理有限公司,陕西 西安 710075;2.长安大学公路学院,陕西 西安 710064; 3.中国铁路兰州局集团有限公司天水车站,甘肃 天水 741000
  • 出版日期:2026-11-03 发布日期:2026-11-10
  • 通讯作者: 纪小平(1982—),男,教授,博士,博士研究生导师。
  • 作者简介:杨永恒(1979—),男,高级工程师,硕士。
  • 基金资助:
    陕西省交通科技项目(编号:23-98k)。

Synergistic Preparation of Fully Solid-Waste Pavement Base Material Using Phosphogypsum-Based Geopolymer and Lightweight Aggregates and Its Durability

YANG Yongheng1 ,MA Jia1 ,DENG Hongliang2,3 ,JI Xiaoping2 ,DONG Liyuan2 ,LI Yongtao1   

  1. 1.Shaanxi Transportation Holding Jiantou Management and Operation Co.,Ltd.,Xi′an 710075,China; 2.School of Highway,Chang′an University,Xi′an 710064,China; 3.Tianshui Station,China Railway Lanzhou Bureau Group Co.,Ltd.,Tianshui 741000,China
  • Online:2026-11-03 Published:2026-11-10

摘要: 为实现磷石膏在路面基层中的高掺量、高值化利用,本研究以磷石膏基地聚合物(PBG)完全替代水泥 作为胶结料,以磷石膏轻质集料(PLA)部分替代天然集料,协同制备全固废磷石膏路面基层材料(PPBM),并系统测 试其水稳定性、抗冻融性能、干燥收缩性能及温度收缩性能。研究结果表明:水稳定性方面,当PBG掺量由8%增至 16%时,浸水13 d水稳定系数(K13 )由71.84%提升至85.13%,16%掺量下可满足基层材料水稳定性技术要求;抗冻融 性能方面,PBG掺量≥8%时,经5次冻融循环后的强度残留比(BDR5 )达67.2%以上,满足中冻区规范要求(BDR≥ 65%),掺量增至16%时BDR5 进一步提升至91.1%;干缩性能方面,干缩应变随PBG掺量增加而显著增大,16%掺量 试件7 d干缩应变较8%掺量增长约1.15倍;温缩性能方面,平均温缩系数随PBG掺量从8%增至16%由6.76× 10-6 /℃升至10.38×10-6 /℃,各掺量下温缩系数峰值均出现在0~-10 ℃低温。与PBG稳定碎石基层相比,PB-SLB水 稳定性与抗干缩性能略低,但在抗冻融(中低掺量)与温缩抗力方面表现更优。综合各项性能,推荐PBG掺量为8%~ 12%,在水分侵蚀风险较高地区宜取12%,寒冷地区取8%即可满足抗冻要求,但需配合抗裂措施控制干缩与温缩变 形。本研究可为磷石膏在路面基层工程中的规模化、高附加值利用提供技术依据与理论支撑。

关键词: 路面基层 , 磷石膏 , 地聚合物 , 轻质集料 , 全固废 , 耐久性

Abstract: To achieve high-volume and high-value utilization of phosphogypsum in pavement base courses,this study completely replaced cement with phosphogypsum-based geopolymer (PBG) as the binder and partially replaced natural aggre gates with phosphogypsum lightweight aggregates (PLA) to collaboratively prepare a fully solid-waste phosphogypsum pave ment base material (PPBM).The water stability,freeze-thaw resistance,drying shrinkage,and temperature shrinkage perform ances were systematically evaluated.The results indicate that∶regarding water stability,the water stability coefficient after 13 days of immersion (K13 ) increased from 71.84% to 85.13% as the PBG content rose from 8% to 16%,meeting the technical requirements for base materials at 16% PBG content.Regarding freeze-thaw resistance,the residual strength ratio after 5 freeze thaw cycles (BDR5 ) exceeded 67.2% when PBG content was ≥8%,satisfying the specification requirement for moderate frost regions (BDR≥65%),and further increased to 91.1% at 16% PBG content.Regarding drying shrinkage,the drying shrinkage strain increased significantly with PBG content,with the 7-day strain at 16% PBG content being approximately 1.15 times that at 8% content.Regarding temperature shrinkage,the average thermal shrinkage coefficient increased from 6.76×10-6 /℃ to 10.38×10-6 /℃ as PBG content increased from 8% to 16%,with peak values occurring within the 0~-10 ℃ low-temperature range across all mixture proportions.Compared with PBG-stabilized crushed stone base,PB-SLB exhibited slightly lower waterstability and drying shrinkage resistance,but demonstrated superior freeze-thaw resistance (at moderate-to-low PBG contents) and temperature shrinkage resistance.Considering the overall performance,the recommended PBG content ranges from 8% to 12%,with 12% preferred in areas with high water erosion risk and 8% sufficient in cold regions,provided that anti-cracking measures are implemented to control drying and temperature shrinkage.This study provides a technical basis and theoretical support for the large-scale and high-value utilization of phosphogypsum in pavement base engineering.

Key words:  pavement base course,phosphogypsum,geopolymer,lightweight aggregate,fully solid-waste,durability

中图分类号: