欢迎访问《金属矿山》杂志官方网站,今天是 分享到:
×

扫码分享

金属矿山 ›› 2008, Vol. 38 ›› Issue (10): 48-51.

• 矿物工程 • 上一篇    下一篇

某提铁降杂独立精选厂的工艺设计与生产实践

罗立群1, 2,方勇3,陈典助4,任瑾荣5,杨新跃5   

  1. 1.武汉理工大学;2.矿物资源加工与环境湖北省重点实验室;3.长沙矿冶研究院;4.长沙有色冶金设计研究院;5.山西奔腾工矿品贸易公司
  • 收稿日期:2008-08-10 出版日期:2008-10-15 发布日期:2011-07-13
  • 基金资助:

    山西省“两区”开发重点项目(编号:2006012079)。

Research & Design of the Beneficiation Process for Separate Quality Improvement & Impurities Reduction of Iron Concentrate and Its Application Practice

Luo Liqun1,2,Fang Yong3,Chen Dianzhu4,Ren Jinrong5,Yang Xinyue5   

  1. 1.Wuhan University of Technology;2.Mineral Resources Processing and Environment Laboratory of Hubei;3.Changsha Research Institute of Mining and Metallurgy;4.Changsha Engineering & Research Institute of Nonferrous Metallurgy;5.Industry and Mining Product Trading Company of Shanxi
  • Received:2008-08-10 Online:2008-10-15 Published:2011-07-13

摘要: 山西某地有着为数众多的磁铁矿小型选厂,产出的弱磁选铁精矿铁品位仅61%~58%、SiO2含量达12%~15%,不符合高炉炼铁的精料方针,严重影响销售。为此,在试验研究的基础上,采用反浮选—中矿再磨—弱磁选工艺及可在常温下进行浮选的高效阴离子捕收剂LP-4,结合当地实际情况设计、建设了对这些弱磁选铁精矿集中进行提铁降杂的独立精选厂。生产实践表明,该独立精选厂工艺流程运行稳定,适应性强,可使最终精矿铁品位达到67.2%~66.5%,SiO2含量降至5.2%~5.8%,提铁降杂效果良好。

关键词: 弱磁选铁精矿, 提铁降杂, 独立精选厂, 反浮选, 高效捕收剂LP-4

Abstract: There are a number of small sized magnetite ore concentrators in a region in Shanxi, which produce iron concentrates by low intensity magnetic separation that have an iron grade of only 61%~58% but an SiO2 content as high as 12%~15%, not conforming to the guideline of good burden preparation for blast furnace iron-making and seriously affecting their sales. Based on the experimental research and in light of the local real conditions, a separate concentrator for their upgrading has been designed and built for a centralized treatment of these iron concentrates, which adopts a process consisting of reverse flotation, middling regrinding and low magnetic separation, and a high efficient anionic collector LP-4 that can be used in normal temperature. Now, this separate concentrator is running stably and has a good adaptability. It is capable to raise the iron grade of the concentrate to 67.2%~66.5%and reduce the SiO2 content to 5.2%~5.8%, demonstrating a good effect of quality improvement and impurity reduction.

Key words: Iron concentrates of low intensity magnetic separation, Quality improvement and impurities reduction, Separate upgrading concentrator, Reverse flotastion, High efficient collector LP-4