Metal Mine ›› 2011, Vol. 40 ›› Issue (03): 74-77.

Previous Articles     Next Articles

Experimental Research on Beneficiation of a Yunnan Scheelite Mine

Lin Rixiao,Zhang Faming,Zeng Qingjun,Chen Zhijie,Zhang Xianhua   

  1. Guangzhou Research Institute of Nonferrous Metals
  • Online:2011-03-10 Published:2011-03-11

Abstract: According to the characteristics of fine-grained disseminated scheelite in run-of-mine, the scheelite was concentrated by adopting the full flotation process with sodium carbonate as regulator agent, sodium silicate as inhibitor for the gangue minerals, and ZL Pharmacy as collector. 32.34% of the coarse scheelite concentrate (WO3) with tungsten recovery of 95.32% was obtained from the raw ores with grade of 1.43%. Through the comparison tests between concentration at normal temperature and heating temperature, it was determined to concentrate the rough tungsten by heating, by which the high-quality scheelite with tungsten (WO3) of 66.16% and tungsten concentrate recovery of 91.78% was obtained.

Key words:  Scheelite, Fine dissemination, Full flotation, Heating concentration