金属矿山 ›› 2013, Vol. 42 ›› Issue (09): 72-75.

• 矿物工程 • 上一篇    下一篇

新疆某高硅低品位赤铁矿石选矿试验

高雅巍1,2,刘成松1,2,李京社1,唐海燕1,2   

  1. 1.钢铁冶金新技术国家重点实验室;2.北京科技大学冶金与生态工程学院
  • 出版日期:2013-09-16 发布日期:2013-11-22

Beneficiation Experiment on a High-silica Low-grade Hematite Ore in Xinjiang

Gao Yawei 1,2,Liu Chengsong 1,2,Li Jingshe 1,Tang Haiyan 1,2   

  1. 1.State Key Laboratory of Advanced Metallurgy;2.School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing
  • Online:2013-09-16 Published:2013-11-22

摘要: 对新疆某高硅低品位难选赤铁矿石采用阶段磨矿、阶段高梯度强磁选—反浮选原则流程进行了开发利用工艺技术条件研究。结果表明,用磨矿—强磁粗选—粗精矿再磨—强磁精选—强磁精矿1粗1精反浮选、精选尾矿返回流程处理,可获得铁品位为61.10%、铁回收率为65.63%的铁精矿。

关键词: 赤铁矿, 强磁选, 反浮选

Abstract: Ore dressing processes consisting of stage grinding-stage high gradient high intensity magnetic separation-reverse flotation were applied for development and utilization of a high-silica low-grade hematte ore in Xinjiang. The results showed that ironc concentrate with Fe grade of 61.10% and Fe recovery of 65.63% was achieved throght the process flowsheet of grinding-high intensity magnetic separation-regrinding of coarse concentrate-clean concentration by high intensity magantic separation-one roughing and one cleaning reverse floatation of the high intensity concentrate-middles back to the flowsheet.

Key words: Hematite, High intensity magnetic separation, Reverse flotation