高效减水剂对全尾砂充填料性能的影响

范作鹏1,任少峰1,张忠辉1,蔡梦茜2,史琛2,何廷树2   

  1. 1.山东黄金矿业(莱州)有限公司焦家金矿,山东 烟台 261441;2.西安建筑科技大学材料与矿资学院,陕西 西安 710055
  • 出版日期:2014-05-15 发布日期:2014-09-11
  • 基金资助:

    * “十二五”国家科技支撑计划项目(编号:2012BAB08B00)。

Effects of Superplasticizers on Properties of Whole Tailing Backfilling Materials

Fan Zuopeng1,Ren Shaofeng1,Zhang Zhonghui1,Cai Mengqian2,Shi Chen2,He Tingshu2   

  1. 1.Jiaojia Gold Mine,Shandong Gold Mining (Laizhou) Co.,Ltd.,Yantai 261441,China;2.College of Materials & Mineral Resources,Xi′an University of Architecture and Technology,Xi′an 710055,China
  • Online:2014-05-15 Published:2014-09-11

摘要: 利用全尾砂作为集料制成全尾砂充填料对采空区进行充填,具有性能优、尾砂利用率高、能耗少、成本低等优点。根据某矿山现有充填工艺,采用全尾砂替代分级尾砂作为充填集料的技术,优化原有的胶结材料,并将尾砂充填料浆的固体浓度由68%提高到72%,结合使用减水剂来实现全尾砂充填料的自流输送。研究4种减水剂(萘系高效减水剂NSF、聚羧酸高效减水剂PC、氨基高效减水剂ASF以及脂肪族高效减水剂SAF)的不同掺量对全尾砂充填料浆的泌水率、流变性能和强度的影响。结果表明,减水剂的加入有效地提高了全尾砂充填料浆的流动性能,延缓了凝结时间,但却对充填体强度有不利的影响。综合4种减水剂的作用来看,在脂肪族减水剂掺量为1.6%时,既可以使料浆流动性增加幅度较大,又对充填体强度的不利影响较小。因此,选用脂肪族减水剂可以配制性能较优的自流型全尾砂充填材料。

关键词: 充填材料, 全尾砂, 高效减水剂, 流变性

Abstract: The mined-out areas were filled with aggregates of whole tailings backfilling materials with excellent performance,high utilization rate of tailings,low energy consumption and low cost.According to the existing filling process of a mine,the aggregate fill technology in which the whole tailings replace the grade tailings can optimize the original cementing material and increase the solid concentration of tailings backfill slurry from 68% to 72%.The self-flowing transportation of whole tailings backfill material can be realized with the combination of superplasticizer.The effects of different dosage of four superplasticizers (naphthalene superplasticizer,polycarboxylate superplasticizer,aminosalfonic superplasticizer and aliphatic amino superplasticizer) on bleeding rate,rheological property,and strength of the whole tailings backfill slurry were investigated.The experiment results showed that the addition of superplasticizers effectively improved flow property and retard setting time,but it was disadvantageous to compressive strength.On the whole,SAF with the content of 1.6% not only substantially increased the flow property but also had little negative effect on compressive strength.SAF is the best superplasticizer to prepare the whole tailings backfilling materials and realize the self-flowing transportation.

Key words: Backfilling materials, Whole tailings, Superplasticizer, Rheological property