司家营铁矿废石选矿工艺研究

陈洲1,2,3,杨任新1,2,3,王炬1,2,3,李俊宁1,2,3,袁启东1,2,3   

  1. 1.中钢集团马鞍山矿山研究院有限公司,安徽 马鞍山 243000;2.华唯金属矿产资源高效循环利用国家工程研究〖〗中心有限公司,安徽 马鞍山 243000;3.金属矿山安全与健康国家重点实验室,安徽 马鞍山 243000
  • 出版日期:2016-02-15 发布日期:2016-03-11

Beneficiation Technology Study on Iron Waste Rock from Sijiaying

Chen Zhou1,2,3,Yang Renxin1,2,3,Wang Ju1,2,3,Li Junning1,2,3,Yuan Qidong1,2,3   

  1. 1.Sinosteel Maanshan Institute of Mining Research Co.,Ltd.,Maanshan 243000,China;2.National Engineering Research Center of Huawei High Efficiency Cyclic Utilization of Metal Mineral Resources Co.,Ltd.,Maanshan 243000,China;3.State Key Laboratory of Safety and Health for Metal Mine,Maanshan 243000,China
  • Online:2016-02-15 Published:2016-03-11

摘要: 针对河北司家营铁矿废石堆存量大、铁品位低、嵌布粒度细、处理难度大的特点,提出采用预选—阶段磨矿—阶段磁选—阴离子反浮选工艺流程处理。结果表明:铁品位为18.79%的废石经永磁干式磁选机抛尾—中细粒高梯度湿式强磁选机抛尾,可以获得铁品位为29.25%、回收率为59.61%的预选精矿,预选精矿经两阶段磨矿—阶段磁选,可以获得铁品位为52.71%、回收率为48.50%的磁选混合精矿,磁选混合精矿以NaOH为pH调整剂、淀粉为抑制剂、CaO为活化剂、MF为反浮选捕收剂,经1粗1精2扫反浮选,获得了铁品位为65.97%、作业回收率为89.21%、对原矿回收率为43.27%的合格精矿,可以为该类废石的资源化利用提供参考。

关键词: 含铁矿废石, 预选, 阶段磨矿阶段磁选, 浮选

Abstract: Aiming at the problems of large volume,low iron grade,fine disseminated,difficult to be separated,process of pre-separation-stage grinding stage magnetic separation magnetic separation-anionic reverse flotation process was put forward on iron waste rock from Sijiaying of Hebei Province.Results show that waste rock with iron grade of 18.79% via discarding by permanent magnet dry magnetic separator-middle and fine wet high gradient high intensity magnetic separator separation,pre-concentrate with iron grade of 29.25% and recovery of 59.61% was obtained,pre-concentrate via two stage grinding stage magnetic separation operation,magnetic mixed concentrate with iron grade of 52.71% and recovery of 48.50% was obtained,using NaOH as pH regulator,starch as depressor,CaO as activator,MF as reverse flotation collector,via one roughing-one cleaning-two scavenging reverse flotation,qualified concentrate with iron grade of 65.97%,yield recovery of 89.21%,the ore recovery rate is 43.27% was obtained,can provide reference for the recycle of the waste rock resources.

Key words: Waste rocks containing iron, Pre-concentration, Stage grinding stage magnetic separation, Flotation