羧酸铵盐浸取剂对风化壳淋积型稀土矿助浸过程研究

陈文斗,张臻悦,池汝安   

  1. 1. 武汉工程大学资源与安全工程学院,湖北 武汉 430073;2. 绿色化工教育部重点实验室,湖北 武汉 430073
  • 出版日期:2020-05-15 发布日期:2020-06-12
  • 基金资助:
    国家自然科学基金项目(编号:21808176,U1802252,51734001),湖北省教育厅科研项目(编号:Q20191503),武汉工程大学科学研究基金项目(编号:18QD57,18QD50)。

Assisted Leaching Process of Weathered Crust Elution-Deposited Rare Earth Ore by Ammonium Carboxylate

Chen Wendou,Zhang Zhenyue,Chi Ru'an   

  1. 1. School of Resource & Safety Engineering, Wuhan Institute of Technology, Wuhan 430073, China; 2. Key Laboratory for Green Chemical Process of Ministry of Education, Wuhan 430073, China
  • Online:2020-05-15 Published:2020-06-12

摘要: 目前,稀土矿浸出研究仅针对稀土浸出过程中抑杂浸出或抑制黏土矿物膨胀的某一方面。为综合考虑稀土浸出过程中高效抑铝和抑制黏土矿物膨胀的协同作用,采用氯化铵分别与不同浓度的乙酸铵、酒石 酸铵、柠檬酸铵3种羧酸铵盐助浸剂组成复配溶液,通过柱浸方法回收风化壳淋积型稀土矿,从而实现在保证稀土浸出率的情况下,达到有效降低浸出液中杂质铝含量的目的,同时得到黏土矿物的最佳抑膨条件。选用 0.2 mol/L氯化铵分别与3种羧酸铵盐助浸剂复配,探讨了助浸剂浓度、浸出温度及浸出液pH对风化壳淋积型稀土矿浸出过程以及对黏土矿物膨胀性能的影响。结果表明,3种羧酸铵盐助浸剂的最佳添加浓度为:0.04 mol/L乙酸铵、0.07 mol/L酒石酸铵、0.005 mol/L柠檬酸铵,在最佳添加剂浓度下抑铝能力为:乙酸铵>柠檬酸铵>酒石酸铵,黏土矿物的膨胀率大小为:δ乙酸铵<δ酒石酸铵<δ柠檬酸铵。在常温下,0.2 mol/L 氯化铵与0.04 mol/L乙酸铵复配溶液作为浸取剂时抑铝和防膨效果最佳,在pH=4时,稀土浸出率为90.08%,铝浸出率为26.37%,黏土矿物膨胀率为2.705%。

关键词: 风化壳淋积型稀土矿, 助浸, 抑铝, 膨胀

Abstract: At present, the study of rare earth leaching only focuses on one aspect of inhibiting the impurity leaching or the swelling of clay minerals in the process of rare earth leaching. In order to comprehensively consider the synergistic effects of high effective aluminum inhibition and clay mineral swelling inhibition during rare earth leaching, leaching agents are composed of ammonium chloride and ammonium acetate, ammonium tartrate, ammonium citrate three ammonium carboxylate assist leaching agent to reduce the leaching efficiency of impurity aluminum and ensure the efficiency of rare earth, at the same time, the best swelling inhibition conditions were obtained. The effects of the assist leaching agent concentration , leaching temperature and solution pH on the leaching process of weathered crust elution-deposited rare earth ore and the swelling properties of clay minerals were also studied while 0.2 mol/L ammonium chloride mixed with the three carboxylic acid ammonium salts. The results showed that the optimal addition concentration of the three ammonium carboxylate were: 0.04 mol/L ammonium acetate, 0.07 mol/L ammonium tartrate, 0.005 mol/L ammonium citrate, the aluminum inhibition capacity was: ammonium acetate>ammonium citrate>ammonium tartrate, and the swelling ratio of clay minerals was: δacetate<δtartrate<δcitrate. At normal temperature, the mixed solution of 0.2 mol/L ammonium chloride and 0.04 mol/L ammonium acetate as the leaching agent had the best effect of aluminum inhibition and swelling inhibition. The optimal pH condition was 4, the leaching efficiency of rare earth was 90.08%, the leaching efficiency of aluminum was 26.37%, and the swelling ratio of clay mineral was 2.705%.

Key words: Weathered crust elution-deposited rare earth ores, Assisted leaching, Aluminum inhibition, Swelling