福建某铅锌浮选尾矿再选试验研究

李 鑫1,2 邓荣东3 王锦荣1,2 陈 钦2 张承杰2 何环银2 林建绥2 刘想想2
  

  1. 1. 福州大学先进制造学院,福建 晋江 362200;2. 中国冶金地质总局第二地质勘查院,福建 福州 350108;3. 福州大学紫金地质与矿业学院,福建 福州 350116
  • 出版日期:2023-03-15 发布日期:2023-04-12

Experiment Research on Reselection of a Lead-Zinc Flotation Tailings in Fujian

LI Xin1,2 DENG Rongdong3 WANG Jinrong1,2 CHEN Qin2 ZHANG Chengjie2 HE Huanyin2LIN Jiansui2 LIU Xiangxiang2   

  1. 1. School of Advanced Manufacturing,Fuzhou University,Jinjiang 362200,China;2. The Second Geological Exploration Institute,China Metallurgical Geology Bureau,Fuzhou 350108,China;3. Zijin School of Geology and Mining,Fuzhou University,Fuzhou 350116,China
  • Online:2023-03-15 Published:2023-04-12

摘要: 福建某铅锌浮选尾矿中铅、锌、银的品位分别为 0. 23%、2. 11%、36. 3 g / t,其中锌和银有较高回收价值。 该尾矿中主要金属矿物为闪锌矿、黄铁矿和方铅矿,非金属矿物以方解石和石英为主。 针对矿石特点,采用优先浮选 开展工艺优化试验。 结果表明:在磨矿细度为-0. 074 mm 占 69. 92%的条件下,以石灰为 pH 调整剂,硫酸锌为抑制 剂,乙硫氮为捕收剂,2#油为起泡剂,经 1 粗 3 精 1 扫浮铅,可获得铅品位 4. 56%、银品位 320 g / t,铅回收率 15. 55%、银 回收率 6. 63%的银铅精矿;针对选铅尾矿,以石灰为 pH 调整剂,硫酸铜为活化剂,丁基黄药为捕收剂,2#油为起泡剂, 经 1 粗 3 精 2 扫浮锌,可获得锌品位 37. 32%、银品位 152 g / t,锌回收率 73. 25%、银回收率 18. 80%的锌精矿。 试验指 标较好,可为该尾矿的综合利用提供数据支撑。

关键词: 铅锌尾矿, 尾矿再选, 铅锌分离, 优先浮选

Abstract: The grades of lead,zinc and silver in a lead-zinc flotation tailings from Fujian are 0. 23%,2. 11% and 36. 3 g / t,respectively,among which zinc and silver have high recovery value. The main metallic minerals in the tailings are sphalerite,pyrite and galena,and the non-metallic minerals are mainly calcite and quartz. According to the characteristics of ore,preferential flotation was used to carry out the process optimization test. The results showed that:under the condition of grinding finness of -0. 074 mm accounting for 69. 92%,using lime as pH regulator,zinc sulfate as inhibitor,ethylthio-nitrogen as collector and 2# oil as foaming agent,silver-lead concentrate with lead grade of 4. 56%,silver grade of 320 g / t and lead recovery rate of 15. 55% and silver recovery rate of 6. 63% can be obtained through one roughing,three cleaning and one scavenging for lead flotation. With lime as pH regulator,copper sulfate as activator,butyl xanthate as collector and 2# oil as foaming agent,zinc concentrate with zinc grade of 37. 32%,silver grade of 152 g / t,zinc recovery rate of 73. 25% and silver recovery rate of 18. 80% was obtained through one roughing,three cleaning and two scavenging for zinc flotation. The test index is good and would provide data support for the comprehensive utilization of the tailings.