Welcome to Metal Mine! Today is Share:
×

扫码分享

Metal Mine ›› 2015, Vol. 44 ›› Issue (03): 187-190.

Previous Articles     Next Articles

Recovery of Coke from Blast Furnace Dust by Combined Process of Flotation and Magnetic Separation

Fu Ganghua1,Wang Hongyang1,Guo Yufeng1,Li Pengfei1,Yang Lu1,Zhou Qikui2   

  1. 1.School of Mineral Processing and Bioengineering,Central South University,Changsha 410083,China;2.Songshan Company Technology Center of Shaoguan Iron & Steel Co.,Ltd,Baosteel Group,Shaoguan 512123,China
  • Online:2015-03-15 Published:2015-07-31

Abstract: In order to high effectively recover and utilize the coke existed in blast furnace dust (BFD),combined process of flotation and magnetic separation was used to treat a BFD containing 4.43% Zn and 18.45% C.The results show that:①With kerosene dosage of 800 g/t,terpenic oil dosage of 200 g/t and sodium silicate dosage of 1 500 g/t,rough coke concentrate with 74.96% C,1.91% Zn,5.19% Fe and carbon recovery of 90.83% was obtained;②Treating magnetite as carrier,coke concentrate with carbon grade of 85.17% and total recovery of 86.29% can be obtained by grinding the flotation concentrate to 74.32% passing 0.074 mm,and then enduring high intensity magnetic separation with 1.5 T background induction intensity,further more the zinc grade in coke concentrate was reduced to 1.29%.The quality of coke concentrate can meet the requirements of matching ore in sintering.

Key words: Blast furnace dust, Coke concentrate, Zinc, Flotation, Magnetic separation