Recovery Test of Scheelite from A Mdybdenum Tailings by Floatathon in Henan

 Liao Dehua1,Chen Xiang2   

  1. 1.Department of Mine Engineering,Liupanshui Normal College;2. Faculty of Resource and Environmental Engineering,Jiangxi University of Science and Technology
  • Online:2012-02-15 Published:2012-05-30

Abstract: In order to recover the scheelite from molybdenum tailings, adopted the process of  pre-classification-+0.15 mm coarse fraction regrinding-one roughing one scavenging flotation desulfurization-one roughing one scavenging one cleaning flotation scheelite under normal temperature-one roughing three scavenging five cleaning heating flotation scheelite, got the tungsten concentrate with grade of WO3 at 60.14%, recovery of WO3 at 77.78%. Coarse fraction regrinding avoids the production of slime and over crushing of scheelite, adding the LY inhibitor can inhibit the gangue containing calcium. These measures ensure the test get better indexes.

Key words: Molybdenum tailing, Recovering scheelite, Heating flotation, Pre-classification, LY inhibitor