摘要: 通过对内蒙古某细粒嵌布萤石矿的浮选试验研究,确定了合理的药剂制度和工艺流程。以自行研制的改性脂肪酸盐YSB-2为捕收剂,在常温(24 ℃)下,采用弱碱性(pH=9.0)1次粗选,弱酸性(pH=6.0)7次精选,精Ⅰ尾矿作为最终尾矿丢弃,其余中矿集中返回到精Ⅰ的碱酸工艺流程,获得了品位为98.70%、回收率为89.20%、SiO2含量为0.93%、CaCO3含量小于0.37%的高品级萤石精矿。

关键词: 细粒嵌布萤石矿, 碱酸浮选工艺, 捕收剂YSB-2

Abstract: A rational reagent regime and process for a finely disseminated fluorite ore from Inner Mongolia were determined through flotation test research.The flotation test adpoted the self-developed modified fatty acid salt YSB-2 as collector and was carried out at a normal temperature (24 ℃).The process was composed of one rougher in weakly alkaline medium(pH=9.0)and seven cleaners in weakly acidic medium (pH=6.0).The tail of cleaner I was the final tail and the middlings were concentrated and returned to the acidic-alkaline process.A high grade fluorite concentrate assaying CaF2 98.70% at a CaF2 recovery of 89.20%, SiO2 0.93% and CaCO3 below 0.37% was produced.