赤泥透水砖的制备及性能研究

李国昌,王萍   

  1. 山东理工大学
  • 出版日期:2009-12-15 发布日期:2011-04-24

Study on Preparation and Performances of the Water Permeable Brick from Red Mud

Li Guochang,Wang Ping     

  1. Shandong University of Technology
  • Online:2009-12-15 Published:2011-04-24

摘要: 以山东铝业公司赤泥为主要原料制备透水砖,并对制品性能的主要影响因素进行了考察。试验结果表明:透水砖骨料的合适配方为赤泥55%,粉煤灰35%,膨润土10%;骨料的烧结温度以1 150 ℃为宜。用该条件下所得骨料制备透水砖的适宜条件为:砖的固体原料中骨料占82%,膨润土占8%,玻璃粉占10%;水玻璃按固体原料的8%添加;砖坯成型压力40 MPa;烧结温度1 080 ℃,烧结时间60 min。制得的赤泥透水砖抗压强度为35.32 MPa,透水系数为0.028 cm/s,磨坑长度为27.35 mm。

关键词: 赤泥, 透水砖, 透水系数, 抗压强度, 耐磨性能

Abstract: The red mud from Shandong Aluminums Company were used to prepare water permeable brick, and then the main factors of affecting the performance of the bricks were investigated. The experiment results showed that the suitable formula for aggregate of the water permeable bricks are red mud of 55%, fly ash 35%, bentonite 10% at an appropriate sintering temperature of 1 150 ℃. Using this aggregate to make the bricks, the appropriate conditions consist of the aggregate of 82% in solid material of bricks, bentonite of 8%, glass powder of 10%, water glass accounting for 8% of solid material at brick molding pressure of 40 MPa, sintering temperature 1 080 ℃, and sintering time 60 min. The compressive strength of red mud water-permeable brick obtained is 35.32 MPa with permeability coefficient of 0.028 cm/s, wear length of 27.35 mm.

Key words: Red mud, Water permeable brick, Permeability coefficient, Compression strength, Abrasion resistance