Abstract: Briefly introduce the technological mineralogy of a refractory oolitic hematite in Hubei province.The experiment was reasearched on the ore of roasting temperature,dosage of reducing agent,roasting time and magnetic intensity.The result showed when the oolitic hematite of 47.57% iron grade was separated by reducing roasting with the roasting temperature of 850 ℃,dosage of 25% powdered carbon,roasting time of 60 min,grinding size of 65%-0.074 mm after quenching and magnetic intensity of 127.39 kA/m,the grade and recovery of iron concentration could reach to 56.75% and 79.96%,respectively.

Key words: Oolitic hematite, Magnetizing roasting, Magnetic separation