Aluminum Reduction Test of a High Alumina Iron Concentrate from Suspension Roasting-Magnetic Separation Abroad

Zhu Yimin1,2,Wang Yan1,2,Zhang Jing2,Gu Xiaotian1,2,Li Yanjun1,2   

  1. 1. College of Resource and Civil Engineering, Northeastern University, Shenyang 110819, China; 2. Technical Engineering Laboratory of High Efficient Exploitation and Utilization of Refractory Iron Ore in Liaoning, Shenyang 110819, China
  • Online:2019-08-15 Published:2019-10-10

Abstract: The content of TFe and Al2O3 in an iron concentrate from suspension roasting-magnetic separation abroad was 64.50% and 5.95% respectively, main iron mineral is magnetite, little hematite. In order to solve the problem of high Al2O3 content in the concentrate, a new type of anionic collector DTL-1 was developed. Aluminium remove experiment was conducted on high-alumina iron concentrate after suspension roasting-magnetic separation via changes of flotation temperature, pH value and the dosage of collector DTL-1. Results indicated that, flotation temperature was 25 ℃, the pH was 8.0 and collector DTL-1 dosage was 50 g/t, through one roughing three cleaning one scavenging closed circuit flotation process, flotation concentrate with TFe grade of 66.40%, TFe recovery of 87.81%, Al2O3 grade of 4.90% was obtained. There is fine-grained alumina minerals wrapped in relatively coarse magnetite particles of flotation iron concentrate products. On the premise of ensuring the recovery of iron, some aluminum-containing iron oxides enter into the iron concentrate, resulting in the high content of aluminum in the iron concentrate.

Key words: High alumina iron ore, Dealumination collector, Flotation performance