Metal Mine ›› 2011, Vol. 40 ›› Issue (10): 91-95.
Previous Articles Next Articles
Liu Limei1,Zhang Yong2
Online:
Published:
Abstract: In order to provide technical basis for rationally developing mineral resources at No.8 ore-body of Benxi Iron and Steel Group in large-scale, and in view of the characteristics of micro-fine embedded magnetite, the beneficiation tests were carried by the process of bulk dry magnetic separation for tailings removal-single low intensity magnetic separation and the process of bulk dry magnetic separation-low intensity magnetic separation-reverse flotation. The results showed that iron concentrate with Fe grade of 65.76% and recovery of 75.93% was obtained by the former under the final grinding fineness -0.030 8 mm 90%;Iron concentrate with Fe grade of 65.47%, recovery of 74.43% was obtained by the latter under the grinding fineness of -0.043 mm 90%. Since the technical indexes obtained by the two processes are similar, which one you adopted depends on the technical and economical comparison.
Key words: No.8 ore-body of Jiajiapuzi iron ore, Micro-fine embedded magnetite, Bulk dry concentration, Low intensity magnetic separation, Reverse flotation
LIU Li-Mei, ZHANG Yong. Research on the Beneficiation Process of No.8 Ore-body of Jiajiapuzi Iron Ore[J]. Metal Mine, 2011, 40(10): 91-95.
/ Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: http://www.jsks.net.cn/EN/
http://www.jsks.net.cn/EN/Y2011/V40/I10/91