Welcome to Metal Mine! Today is Share:
×

扫码分享

Metal Mine ›› 2016, Vol. 45 ›› Issue (06): 86-89.

Previous Articles     Next Articles

Beneficiation Experiment on Fluorite Recovery of Lead-Zinc Tailing from Hunan

Jiang Xiangwei,Guo Yanzhe,Liu Runqing,Jiang Wei,Liu Hang,Sun Wei   

  1. School of Minerals Processing and Bioengineering,Central South University,Changsha 410083,China
  • Online:2016-06-15 Published:2016-08-19

Abstract: There is 18.58% CaF2 in a lead-zinc mined tailings from Hunan,the main impurity composition is SiO2 and CaCO3.In order to provide the basis of the fluorite recovery and utilization of tailings,beneficiation experiment was conducted on the ore.The results indicated that,CDG100 mm×100 mm cycle pulsating high intensity magnetic separator was used to remove iron,non magnetic products with Na2CO3 as regulator,Na2S and sodium silicate as inhibitor,acidification sodium silicate (ratio of sulphunic acid to sodium silicate is 2∶1) as depressor for cleaning,Z-202 as collector,by one roughing,seven cleaning,one scavenging closed circuit flotation test process,fluorite concentrate with CaF2 grade of 94.76%,recovery rate is 53.83% was obtained.Test results can provide technical guidance for comprehensive utilization of lead-zinc mined tailings containing fluorite.

Key words: Tailings containing fluorite, Iron removal by magnetic separation, Flotation